In the preform injection molding process, the whitening of the bottom of the preform is a common problem. The causes and solutions are as follows:

Causes:

‌1. Insufficient hot runner temperature‌: When the hot runner temperature is insufficient, the bottom of the preform may not be fully heated, resulting in whitening.
2. Insufficient material temperature: Insufficient temperature of the injection molding material will also affect the molding quality of the bottom of the preform, causing whitening.
3. High moisture content of the raw material: The moisture in the raw material may evaporate during the injection molding process, resulting in white mist at the bottom of the preform.
4. Uneven cooling: Too fast or too slow cooling water flow rate, or uneven distribution of the cooling system, may lead to uneven temperature at the bottom of the preform, resulting in whitening.

 

Solution:

‌1. Strengthen insulation measures‌: Ensure that insulation measures around the hot runner are in place, reduce heat loss, and increase the temperature of the hot runner.
‌2. Increase the temperature of the hot nozzle‌: Appropriately increase the temperature of the hot nozzle so that the bottom of the bottle preform can be fully heated to avoid whitening.
‌3. Increase the material temperature‌: Increase the temperature of the injection molding material within a reasonable range to ensure that the material can be fully plasticized during the injection molding process.
‌4. Speed up the injection speed‌: Properly speeding up the injection speed can help the material fill the mold better and reduce the whitening phenomenon.
‌5. Reduce the holding pressure‌: Properly reducing the holding pressure can help reduce the stress inside the preform, thereby avoiding whitening.
‌6. Adjust the cooling water flow rate‌: Adjust the cooling water flow rate according to the actual situation to ensure that the bottom of the preform is cooled evenly to avoid whitening caused by uneven temperature.

In summary, solving the problem of whitening at the bottom of the preform requires multiple approaches, including strengthening heat insulation, increasing nozzle temperature, increasing material temperature, accelerating injection speed, reducing holding pressure, and adjusting cooling water flow rate. By using these methods in combination, the molding quality of the bottom of the preform can be effectively improved and the whitening phenomenon can be avoided.