How to solve the problem of silver streaks or yellowing of preforms in the preform injection molding process?

 

page-800-800

 

In the preform injection molding process, silver streaks or yellowing of the preform are common problems, which may be caused by a variety of factors.

The main reasons for silver streaks or yellowing of the preform include:

1. Plastic decomposition: The raw materials may decompose during the injection molding process due to excessive temperature, long time residence or improper screw design, producing gas and impurities, thereby forming silver streaks on the surface of the preform or causing yellowing.
2. Mold problems: mold exhaust poor, large friction resistance of runners, gates, and cavities, or unreasonable cooling systems may cause local overheating of the preform, silver streaks or yellowing.
3. Improper setting of injection molding machine parameters: Improper adjustment of parameters such as temperature and speed of the injection molding machine, such as injection speed fast, material temperature high or hot nozzle temperature high, may also cause quality problems of bottle preforms.
4. Raw material problems: poor quality, impurities or insufficient drying of raw materials may cause silver streaks or yellowing of the preform during the injection molding process.

The following solutions can be adopted for these problems:

1. Optimize the parameters of the injection molding machine: According to the process and raw material characteristics, appropriately adjust the temperature, speed and other parameters of the injection molding machine to ensure that the plastic melt does not overheat or stay for too long during the processing.
2. Improve mold design: optimize the exhaust system of the mold, reduce the friction resistance of the runner, gate, and cavity, ensure a reasonable cooling system, and avoid local overheating of the preform.
3. Strengthen raw material management: Select high-quality raw materials for injection molding preforms to ensure the purity and quality of the raw materials. Fully dry the raw materials before injection molding to avoid excessive moisture or impurities in the raw materials.
4. Regularly maintain the mold: Check and clean the mold regularly to ensure that the mold surface is clean and smooth to reduce the impact on the raw materials.

In summary, the problem of silver streaks or yellowing of preforms in the preform injection molding process can be effectively solved by optimizing injection molding machine parameters, improving mold design, strengthening raw material management and regularly maintaining molds.